PIG IRON
Pig iron is an iron-carbon alloy with a carbon content of more than 2%. Industrial pig iron generally has a carbon content of 2.11% -4.3%, and contains elements such as C, Si, Mn, S, and P. It is smelted with iron ore in a blast furnace product.
Pig iron performance is hard, wear-resistant, and good castability , but pig iron is brittle and cannot be forged.
Mingda Metal has been in Pig Iron field for many years,till now we have source from China,India,Brazil,South Africa,Russia,etc..
Chemicals Composition
SPECS |
Chemicals Composition(%) |
Carbon |
Silicon |
Manganese |
Phosphor |
Sulphur |
Min% |
Max% |
Ductile pig iron Ex China (FCD) |
3.5 |
1.2 |
0.2 |
0.06 |
0.03 |
Foundry Pig iron Ex China (FC) |
3.5 |
1.5-1.8% |
0.3 |
0.06 |
0.03 |
Foundry Pig iron Ex China (FC) |
3.5 |
1.8-2.2% |
0.3 |
0.06 |
0.03 |
Foundry Pig iron Ex China (FC) |
3.8 |
1.5-2.2% |
0.5-1.0% |
0.1 |
0.06 |
Foundry pig iron Ex India (FC) |
3.5 |
1.6-2.0% |
0.5-0.9% |
0.15 |
0.06 |
Foundry pig iron Ex India (FC) |
3.5 |
2.0-2.5% |
0.5-0.9% |
0.15 |
0.06 |
Nodular Pig Iron Ex Brazil |
3.5-4.5% |
0.50 |
0.08 |
0.08 |
0.02 |
Nodular Pig Iron Ex Brazil |
3.5-4.5% |
0.5-1.0 |
0.08 |
0.08 |
0.02 |
Grey Pig Iron Ex Brazil |
3.5-4.5% |
1.5-2.0% |
0.7 |
0.10 |
0.03 |
Grey Pig Iron Ex Brazil |
3.5-4.5% |
2.0-2.5% |
0.7 |
0.10 |
0.03 |
Basic Pig Iron Ex Russia |
3.8-4.8% |
1.2 |
0.2 |
0.07 |
0.035 |
Size |
2-9kgs ,2-15kgs, 90% Min |
Packing |
In 1mt jumbo bag,In bulk In 20'GP |
Supply Ability:
3000 Tons per Month
Quality Control:
Certificate Of Quality issued by our factory or The Third Party.
Lead Time :
Quantity(Tons) |
1 - 20 |
21 - 100 |
101 - 500 |
>500 |
Est. Time(days) |
3 |
7 |
15 |
To be negotiate |
Welcome contact us as follows:
UPET GROUP CO.,LTD
Contact:Lisa